Teflon® PFA 345
全氟烷氧基
DuPont Fluoropolymers
产品说明:
For inventory control purposes product name may be followed by an X.
Products labeled PFA 345 and PFA 345 X are equivalent and all information in this document is applicable to both.
Typical Application
Applications for DuPont™ Teflon ® PFA 345 include extruded tubing, wire and cable insulation, injection molded parts, and chemically resistant linings for bellows, valves, fittings, pipes, pumps, and other fluid-handling components.
Description
DuPont™ Teflon ® PFA 345 is a medium melt flow rate fluoroplastic resin available in pellet form. Compared with Teflon ® PFA 340, it offers increased flex life and greater resistance to environmental stress-cracking (Teflon ® PFA 345 offers a typical MIT folding endurance of 50,000* compared to 15,000 in Teflon ® PFA 340). Table 1 shows the typical property data for Teflon ® PFA 345.
Teflon ® PFA 345 is used when traditional extrusion and molding processes are required for producing products with the superior properties of a fluoroplastic resin. Compared to other thermoplastics, the high melt strength and thermal stability of Teflon ® PFA 345 can be used to improve processing rates. Compared with other fluoroplastics, creep resistance at high service temperatures provides a superior balance and level of end-use properties. Teflon ® PFA 345 combines the processing ease of conventional thermoplastics with many properties similar to those of polytetrafluoroethylene.
Properly processed products made from neat Teflon® PFA 345 resin provide the superior properties characteristic of fluoroplastic resins: chemical inertness, exceptional dielectric properties, heat resistance, toughness and flexibility, low coefficient of friction, non-stick characteristics, negligible moisture absorption, low flammability, performance at temperature extremes, and excellent weather resistance.
In a flame situation, products of Teflon ® PFA 345 resist ignition and do not promote flame spread. When ignited by flame from other sources, their contribution of heat is very small and added at a slow rate with very little smoke.
Teflon ® PFA 345 meets the requirements of ASTM D3307, Type III
Products labeled PFA 345 and PFA 345 X are equivalent and all information in this document is applicable to both.
Typical Application
Applications for DuPont™ Teflon ® PFA 345 include extruded tubing, wire and cable insulation, injection molded parts, and chemically resistant linings for bellows, valves, fittings, pipes, pumps, and other fluid-handling components.
Description
DuPont™ Teflon ® PFA 345 is a medium melt flow rate fluoroplastic resin available in pellet form. Compared with Teflon ® PFA 340, it offers increased flex life and greater resistance to environmental stress-cracking (Teflon ® PFA 345 offers a typical MIT folding endurance of 50,000* compared to 15,000 in Teflon ® PFA 340). Table 1 shows the typical property data for Teflon ® PFA 345.
Teflon ® PFA 345 is used when traditional extrusion and molding processes are required for producing products with the superior properties of a fluoroplastic resin. Compared to other thermoplastics, the high melt strength and thermal stability of Teflon ® PFA 345 can be used to improve processing rates. Compared with other fluoroplastics, creep resistance at high service temperatures provides a superior balance and level of end-use properties. Teflon ® PFA 345 combines the processing ease of conventional thermoplastics with many properties similar to those of polytetrafluoroethylene.
Properly processed products made from neat Teflon® PFA 345 resin provide the superior properties characteristic of fluoroplastic resins: chemical inertness, exceptional dielectric properties, heat resistance, toughness and flexibility, low coefficient of friction, non-stick characteristics, negligible moisture absorption, low flammability, performance at temperature extremes, and excellent weather resistance.
In a flame situation, products of Teflon ® PFA 345 resist ignition and do not promote flame spread. When ignited by flame from other sources, their contribution of heat is very small and added at a slow rate with very little smoke.
Teflon ® PFA 345 meets the requirements of ASTM D3307, Type III
Teflon® PFA 345 物性表
| 基本信息 | |
|---|---|
| 特性 |
|
| 用途 |
|
| 形式 |
|
| 加工方法 |
|
| 物理性能 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| 比重 | 2.14 | g/cm³ | ASTM D792 |
| 熔流率(熔体流动速率) (372°C/5.0 kg) | 5.0 | g/10 min | ASTM D3307, ISO 12086 |
| 吸水率 (24 hr) | < 0.030 | % | ASTM D570 |
| 硬度 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| 肖氏硬度 (邵氏 D) | 55 | ASTM D2240, ISO 868 |
| 机械性能 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| 抗张强度 (23°C) | 29.0 | MPa | ASTM D3307, ISO 12086 |
| 伸长率 (断裂, 23°C) | 300 | % | ASTM D3307, ISO 12086 |
| 弯曲模量 (23°C) | 551 | MPa | ASTM D790, ISO 178 |
| 热性能 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| 熔融温度 | 305 | °C | ASTM D4591 |
| 电气性能 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| 体积电阻率 | 1.0E+18 | ohms·cm | ASTM D257, ISO 1325 |
| 介电强度 | |||
| 0.250 mm 1 | 80 | kV/mm | ASTM D149 |
| 0.250 mm | 80 | kV/mm | IEC 60243-1 |
| 介电常数 (1 MHz) | 2.03 | ASTM D150, IEC 60250 | |
| 耗散因数 (1 MHz) | < 2.0E-4 | ASTM D150, IEC 60250 |
| 可燃性 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| UL 阻燃等级 2 | V-0 | UL 94 | |
| 极限氧指数 | > 95 | % | ASTM D2863, ISO 4589-2 |
| 补充信息 | 额定值 | 单位制 | 测试方法 |
|---|---|---|---|
| Critical Shear Rate (372°C) | 21.0 | sec^-1 | |
| MIT Folding Endurance 3(200.0 µm) | 5.0E+4 | Cycles | ASTM D2176 |
亲,如果要PDF物性表,可以到物性下载栏目下载,或发邮件到:tjh@rjplastics.com索取!
温馨提示:仁捷公司免费24小时提供塑胶原料注塑成型技术支持,咨询热线:18681139818,联系人:唐生
Tag: PFA ,345